Fluidity of a molten alloy during sand casting depends on its solidification range. The phase diagram of a hypothetical binary alloy of components A and B is shown in the figure with its eutectic composition and temperature. All the lines in this phase diagram, including the solidus and liquidus lines, are straight lines. If this binary alloy with of B is poured into a mould at a pouring temperature of , then the solidification range is

Figure 1 for GATE 2022 ME Set 2 question 19
  1. A

  2. B

  3. C

  4. D

GATE 2022 · Mechanical Engineering · Set 2 · IIT Kharagpur

Answer
(D)

From the official answer key published by IIT Kharagpur.

Worked solution

The solidification range is defined as the temperature difference between the liquidus temperature () and the solidus temperature () for a given alloy composition:

From the phase diagram:
1. The liquidus line connecting pure component A at and the eutectic point at is linear. Its equation is:

For :

2. For a hypoeutectic alloy with (which is greater than the maximum solid solubility of ), solidification completes at the eutectic temperature:

Therefore, the solidification range is:

Note that the pouring temperature of only provides superheat and does not alter the solidification range.

Answer: (D)

Practise Phase Diagrams and Heat Treatment

19 GATE questions from this chapter, in short untimed sets, with the formula sheet beside them. Free.

More from Phase Diagrams and Heat Treatment

Question from the official GATE 2022 ME paper (Set 2), IIT Kharagpur. Solutions by PARIXO AI. All 65 questions of this paper.