GATE 2024 ME · Question 29
The “Earing” phenomenon in metal forming is associated with
- A
deep drawing
- B
rolling
- C
extrusion
- D
forging
GATE 2024 · Mechanical Engineering · IISc Bangalore
Answer
From the official answer key published by IISc Bangalore.
Worked solution
During the deep drawing of sheet metals, planar anisotropy in the sheet (variation of properties along different directions in the sheet plane, characterized by ) leads to non-uniform deformation along the circumference of the drawn cup. This results in the formation of wavy, scalloped edges at the top rim of the cup, a defect specifically known as earing.
Rolling induces this directional anisotropy (crystallographic texture), but the earing defect itself physically manifests during the deep drawing process when the flat circular blank is drawn into a cylindrical cup.
Answer: (A) deep drawing
Practise Sheet Metal Forming Processes
9 GATE questions from this chapter, in short untimed sets, with the formula sheet beside them. Free.
More from Sheet Metal Forming Processes
- GATE 2024 ME · Q62A blanking operation is performed on C20 steel sheet to obtain a circular disc having a diameter of 20 mm…
- GATE 2020 ME Set 1 · Q32A sheet metal with a stock hardness of 250 HRC has to be sheared using a punch and a die having a clearance…
- GATE 2018 ME Set 1 · Q46The percentage scrap in a sheet metal blanking operation of a continuous strip of sheet metal as shown in…
- GATE 2017 ME Set 1 · Q48A 10 mm deep cylindrical cup with diameter of 15 mm is drawn from a circular blank. Neglecting the variation…
- GATE 2016 ME Set 3 · Q60In a sheet metal of 2 mm thickness a hole of 10 mm diameter needs to be punched. The yield strength in…
- GATE 2014 ME Set 2 · Q65A rectangular hole of size 100 mm × 50 mm is to be made on a 5 mm thick sheet of steel having ultimate…
Question from the official GATE 2024 ME paper, IISc Bangalore. Solutions by PARIXO AI. All 65 questions of this paper.