PARIXO GATE · ME Open the app

GATE 2025 ME · Question 20

1 markMultiple choiceManufacturing EngineeringPhase Diagrams and Heat Treatment

Among the following surface hardening processes, steel is heated to the lowest temperature in

  1. A

    carburizing

  2. B

    cyaniding

  3. C

    nitriding

  4. D

    carbonitriding

GATE 2025 · Mechanical Engineering · IIT Roorkee

Answer
(C)

From the official answer key published by IIT Roorkee.

Worked solution

The typical processing temperatures for the given thermochemical surface-hardening treatments of steel are:

  • Carburizing: Conducted in the austenitic range, typically between and .
  • Cyaniding: Typically carried out in a molten salt bath between and .
  • Carbonitriding: An austenitic diffusion process conducted between and .
  • Nitriding: Conducted in the ferritic region (below the eutectoid temperature ), typically between and .

Because nitriding occurs in the ferritic state without phase transformation, it requires the lowest temperature among the options, which also minimizes thermal distortion and cracking.

Answer: (C) nitriding

Practise Phase Diagrams and Heat Treatment

19 GATE questions from this chapter, in short untimed sets, with the formula sheet beside them. Free.

More from Phase Diagrams and Heat Treatment

Question from the official GATE 2025 ME paper, IIT Roorkee. Solutions by PARIXO AI. All 65 questions of this paper.