GATE 2026 ME · Question 59
In a deep drawing operation of a rectangular sheet metal, stretching in length results in reduction in thickness. Assuming volume constancy, the normal anisotropy of the sheet metal is ________ *(rounded off to 2 decimal places)*.
GATE 2026 · Mechanical Engineering · IIT Guwahati
Answer
From the official answer key published by IIT Guwahati.
Worked solution
Normal anisotropy (-value) is defined as the ratio of true plastic strain in the width direction to that in the thickness direction:
Given an increase in length of () and a reduction in thickness of ():
By volume constancy during plastic deformation, :
Therefore, the normal anisotropy is:
Answer: 0.61
Practise Sheet Metal Forming Processes
9 GATE questions from this chapter, in short untimed sets, with the formula sheet beside them. Free.
More from Sheet Metal Forming Processes
- GATE 2024 ME · Q29The “Earing” phenomenon in metal forming is associated with
- GATE 2024 ME · Q62A blanking operation is performed on C20 steel sheet to obtain a circular disc having a diameter of 20 mm…
- GATE 2020 ME Set 1 · Q32A sheet metal with a stock hardness of 250 HRC has to be sheared using a punch and a die having a clearance…
- GATE 2018 ME Set 1 · Q46The percentage scrap in a sheet metal blanking operation of a continuous strip of sheet metal as shown in…
- GATE 2017 ME Set 1 · Q48A 10 mm deep cylindrical cup with diameter of 15 mm is drawn from a circular blank. Neglecting the variation…
- GATE 2016 ME Set 3 · Q60In a sheet metal of 2 mm thickness a hole of 10 mm diameter needs to be punched. The yield strength in…
Question from the official GATE 2026 ME paper, IIT Guwahati. Solutions by PARIXO AI. All 65 questions of this paper.