A butt weld joint is developed on steel plates having yield and ultimate tensile strength of and , respectively. The thickness of the plates is and width is . Improper selection of welding parameters caused an undercut of depth along the weld. The maximum transverse tensile load (in ) carrying capacity of the developed weld joint is _______

GATE 2014 · Mechanical Engineering · Set 4 · IIT Kharagpur · printed as Q.55 in the ME section

Answer
68 to 72

From the official answer key published by IIT Kharagpur.

Worked solution

The maximum load-carrying capacity of a tensile member is governed by the ultimate tensile strength () of the material and the minimum (critical) cross-sectional area available to resist the load.

Given:

  • Plate thickness,
  • Plate width,
  • Depth of undercut,
  • Yield strength,
  • Ultimate tensile strength,

Due to the undercut along the length of the weld, the effective thickness of the joint is reduced to:

The effective cross-sectional area resisting the transverse tensile load is:

The maximum transverse tensile load carrying capacity corresponds to the ultimate strength:

Answer: 70

Practise Welded Joints

5 GATE questions from this chapter, in short untimed sets, with the formula sheet beside them. Free.

More from Welded Joints

Question from the official GATE 2014 ME paper (Set 4), IIT Kharagpur. Solutions by PARIXO AI. All 65 questions of this paper.