The "Jominy test" is used to find

  1. A

    Young's modulus

  2. B

    hardenability

  3. C

    yield strength

  4. D

    thermal conductivity

GATE 2016 · Mechanical Engineering · Set 1 · IISc Bangalore · printed as Q.20 in the ME section

Answer
(B)

From the official answer key published by IISc Bangalore.

Worked solution

The Jominy end-quench test is a standardized method used to determine the hardenability of an alloy steel.

In this test:
1. A standard cylindrical specimen of diameter () and length () is austenitized uniformly.
2. It is quickly placed in a fixture and quenched at one end by a controlled jet of water.
3. The cooling rate decreases along the length away from the quenched end.
4. Rockwell C hardness () is measured along flat surfaces ground along the length at regular intervals.

The resulting hardness versus distance curve demonstrates the depth to which the steel can be hardened, which defines its hardenability.

Answer: (B) hardenability

Practise Phase Diagrams and Heat Treatment

19 GATE questions from this chapter, in short untimed sets, with the formula sheet beside them. Free.

More from Phase Diagrams and Heat Treatment

Question from the official GATE 2016 ME paper (Set 1), IISc Bangalore. Solutions by PARIXO AI. All 65 questions of this paper.