GATE 2019 ME Set 1 · Question 23
1 markMultiple choiceManufacturing EngineeringCasting: Patterns, Moulds, Gating and Solidification
In a casting process, a vertical channel through which molten metal flows downward from pouring basin to runner for reaching the mold cavity is called
- A
blister
- B
sprue
- C
riser
- D
pin hole
GATE 2019 · Mechanical Engineering · Set 1 · IIT Madras · printed as Q.13 in the ME section
Answer
(B)
From the official answer key published by IIT Madras.
Worked solution
In metal casting, the elements of the gating system serve specific functions:
- Pouring basin: A reservoir that receives molten metal from the ladle to minimize turbulence.
- Sprue: A tapered vertical channel through which the molten metal flows downward from the pouring basin to the runner under gravity.
- Runner: A horizontal distribution channel that carries molten metal from the sprue base toward the ingates.
- Ingate: The opening through which the molten metal enters the mold cavity.
- Riser: A reservoir provided in the mold to feed liquid metal to the casting to compensate for liquid and solidification shrinkage.
"Blister" and "pin hole" are types of casting defects rather than gating components.
Answer: (B) sprue
Practise Casting: Patterns, Moulds, Gating and Solidification
34 GATE questions from this chapter, in short untimed sets, with the formula sheet beside them. Free.
More from Casting: Patterns, Moulds, Gating and Solidification
- GATE 2019 ME Set 1 · Q47Match the following sand mold casting defects with their respective causes. | Defect | Cause | | :--- | :---…
- GATE 2019 ME Set 2 · Q25The fluidity of molten metal of cast alloys (without any addition of fluxes) increases with increase in
- GATE 2019 ME Set 2 · Q60The figure shows a pouring arrangement for casting of a metal block. Frictional losses are negligible. The…
- GATE 2018 ME Set 2 · Q23During solidification of a pure molten metal, the grains in the casting near the mould wall are
- GATE 2018 ME Set 2 · Q60For sand-casting a steel rectangular plate with dimensions 80 mm × 120 mm × 20 mm, a cylindrical riser has…
- GATE 2017 ME Set 1 · Q54A sprue in a sand mould has a top diameter of 20 mm and height of 200 mm. The velocity of the molten metal…
Question from the official GATE 2019 ME paper (Set 1), IIT Madras. Solutions by PARIXO AI. All 65 questions of this paper.