GATE 2019 ME Set 1 · Question 47
Match the following sand mold casting defects with their respective causes.
| Defect | Cause |
| :--- | :--- |
| P Blow hole | 1 Poor collapsibility |
| Q Misrun | 2 Mold erosion |
| R Hot tearing | 3 Poor permeability |
| S Wash | 4 Insufficient fluidity |
- A
P-4, Q-3, R-1, S-2
- B
P-3, Q-4, R-2, S-1
- C
P-2, Q-4, R-1, S-3
- D
P-3, Q-4, R-1, S-2
GATE 2019 · Mechanical Engineering · Set 1 · IIT Madras · printed as Q.37 in the ME section
Answer
From the official answer key published by IIT Madras.
Worked solution
The causes of the given casting defects are:
- Blow hole (P): Trapped gases and steam cannot escape from the mold cavity due to poor permeability of the molding sand 3.
- Misrun (Q): The molten metal fails to completely fill the mold cavity before solidifying due to insufficient fluidity (e.g., low pouring temperature) 4.
- Hot tearing (R): Internal stresses develop during solidification and contraction because the mold or core cannot collapse freely, caused by poor collapsibility 1.
- Wash (S): Mold sand is eroded and carried away by the high-velocity stream of molten metal, leading to excess metal and sand inclusions, which is direct mold erosion 2.
This gives the match: P-3, Q-4, R-1, S-2.
Answer: (D) P-3, Q-4, R-1, S-2
Practise Casting: Patterns, Moulds, Gating and Solidification
34 GATE questions from this chapter, in short untimed sets, with the formula sheet beside them. Free.
More from Casting: Patterns, Moulds, Gating and Solidification
- GATE 2019 ME Set 2 · Q25The fluidity of molten metal of cast alloys (without any addition of fluxes) increases with increase in
- GATE 2019 ME Set 2 · Q60The figure shows a pouring arrangement for casting of a metal block. Frictional losses are negligible. The…
- GATE 2018 ME Set 2 · Q23During solidification of a pure molten metal, the grains in the casting near the mould wall are
- GATE 2018 ME Set 2 · Q60For sand-casting a steel rectangular plate with dimensions 80 mm × 120 mm × 20 mm, a cylindrical riser has…
- GATE 2017 ME Set 1 · Q54A sprue in a sand mould has a top diameter of 20 mm and height of 200 mm. The velocity of the molten metal…
- GATE 2016 ME Set 1 · Q32The part of a gating system which regulates the rate of pouring of molten metal is
Question from the official GATE 2019 ME paper (Set 1), IIT Madras. Solutions by PARIXO AI. All 65 questions of this paper.