Endurance limit of a beam subjected to pure bending decreases with
- A
decrease in the surface roughness and decrease in the size of the beam
- B
increase in the surface roughness and decrease in the size of the beam
- C
increase in the surface roughness and increase in the size of the beam
- D
decrease in the surface roughness and increase in the size of the beam
GATE 2019 · Mechanical Engineering · Set 2 · IIT Madras · printed as Q.8 in the ME section
Answer
From the official answer key published by IIT Madras.
Worked solution
The actual endurance limit () of a component is determined from the standard endurance limit () of a polished test specimen using Marin modifying factors:
where:
- is the surface condition factor: rougher surfaces have higher stress concentrations (micro-notches), reducing and hence lowering the endurance limit.
- is the size factor: a larger cross-section has a greater volume of material subjected to high stress, increasing the statistical probability of a fatal flaw or defect. Consequently, for larger sizes, which decreases the endurance limit.
Therefore, the endurance limit decreases with an increase in surface roughness and an increase in beam size.
Answer: (C)
Practise Design for Dynamic Loading & Fatigue
19 GATE questions from this chapter, in short untimed sets, with the formula sheet beside them. Free.
More from Design for Dynamic Loading & Fatigue
- GATE 2018 ME Set 2 · Q31Fatigue life of a material for a fully reversed loading condition is estimated from σa = 1100 N-0.15, where…
- GATE 2018 ME Set 2 · Q48A bar is subjected to a combination of a steady load of 60 kN and a load fluctuating between -10 kN and 90…
- GATE 2017 ME Set 1 · Q43A machine element has an ultimate strength (σu) of 600 N/mm2, and endurance limit (σen) of 250 N/mm2. The…
- GATE 2017 ME Set 2 · Q11A machine component made of a ductile material is subjected to a variable loading with σ = -50 MPa and σ =…
- GATE 2016 ME Set 2 · Q48In a structural member under fatigue loading, the minimum and maximum stresses developed at the critical…
- GATE 2015 ME Set 1 · Q29Which one of the following is the most conservative fatigue failure criterion?
Question from the official GATE 2019 ME paper (Set 2), IIT Madras. Solutions by PARIXO AI. All 65 questions of this paper.