GATE 2022 ME Set 1 · Question 29
Which of the following methods can improve the fatigue strength of a circular mild steel (MS) shaft?
- A
Enhancing surface finish
- B
Shot peening of the shaft
- C
Increasing relative humidity
- D
Reducing relative humidity
GATE 2022 · Mechanical Engineering · Set 1 · IIT Kharagpur
Answer
From the official answer key published by IIT Kharagpur.
Worked solution
Fatigue failure predominantly initiates from surface micro-cracks and stress concentrations caused by surface roughness, residual tensile stresses, and environmental corrosion.
- (A) Enhancing surface finish: Smoother surfaces reduce microscopic stress raisers and notches where fatigue cracks initiate, thereby increasing the endurance limit and fatigue strength.
- (B) Shot peening of the shaft: Bombarding the surface with small spherical media induces beneficial compressive residual stresses in the surface layer, which retard crack initiation and propagation.
- (D) Reducing relative humidity: Lower relative humidity decreases atmospheric moisture and corrosive action (corrosion fatigue), slowing down pit formation and crack growth. Conversely, increasing relative humidity (C) promotes corrosion and reduces fatigue strength.
Therefore, options (A), (B), and (D) improve fatigue strength.
Answer: (A) Enhancing surface finish; (B) Shot peening of the shaft; (D) Reducing relative humidity
Practise Design for Dynamic Loading & Fatigue
19 GATE questions from this chapter, in short untimed sets, with the formula sheet beside them. Free.
More from Design for Dynamic Loading & Fatigue
- GATE 2021 ME Set 1 · Q64A machine part in the form of cantilever beam is subjected to fluctuating load as shown in the figure. The…
- GATE 2021 ME Set 2 · Q65The figure shows the relationship between fatigue strength (S) and fatigue life (N) of a material. The…
- GATE 2020 ME Set 2 · Q31A machine member is subjected to fluctuating stress σ = σ0 (8π t). The endurance limit of the material is…
- GATE 2019 ME Set 1 · Q32During a high cycle fatigue test, a metallic specimen is subjected to cyclic loading with a mean stress of…
- GATE 2019 ME Set 2 · Q18Endurance limit of a beam subjected to pure bending decreases with
- GATE 2018 ME Set 2 · Q31Fatigue life of a material for a fully reversed loading condition is estimated from σa = 1100 N-0.15, where…
Question from the official GATE 2022 ME paper (Set 1), IIT Kharagpur. Solutions by PARIXO AI. All 65 questions of this paper.