GATE 2014 ME Set 3 · Question 32
Match the casting defects (Group A) with the probable causes (Group B):
| Group A | Group B |
| :--- | :--- |
| P: Hot tears | 1: Improper fusion of two streams of liquid metal |
| Q: Shrinkage | 2: Low permeability of the sand mould |
| R: Blow holes | 3: Volumetric contraction both in liquid and solid stage |
| S: Cold Shut | 4: Differential cooling rate |
- A
P-1, Q-3, R-2, S-4
- B
P-4, Q-3, R-2, S-1
- C
P-3, Q-4, R-2, S-1
- D
P-1, Q-2, R-4, S-3
GATE 2014 · Mechanical Engineering · Set 3 · IIT Kharagpur · printed as Q.22 in the ME section
Answer
From the official answer key published by IIT Kharagpur.
Worked solution
Matching the casting defects with their underlying causes:
- P. Hot tears (4): Occur due to severe internal stresses caused by differential cooling rates and hindered contraction during solidification.
- Q. Shrinkage (3): Caused by the volumetric contraction of liquid metal and solidifying metal during cooling, especially when risers are inadequate.
- R. Blow holes (2): Internal or surface cavities caused by entrapped gases when the sand mould has low permeability or excessive moisture.
- S. Cold shut (1): A line of discontinuity formed by the imperfect fusion of two streams of converging molten metal that meet at too low a temperature.
Therefore, the correct match is P-4, Q-3, R-2, S-1.
Answer: (B)
Practise Casting: Patterns, Moulds, Gating and Solidification
34 GATE questions from this chapter, in short untimed sets, with the formula sheet beside them. Free.
More from Casting: Patterns, Moulds, Gating and Solidification
- GATE 2014 ME Set 3 · Q35The hot tearing in a metal casting is due to
- GATE 2014 ME Set 3 · Q62A cylindrical blind riser with diameter d and height h, is placed on the top of the mold cavity of a closed…
- GATE 2014 ME Set 4 · Q63A cylindrical riser of 6 cm diameter and 6 cm height has to be designed for a sand casting mould for…
- GATE 2013 ME · Q16A cube shaped casting solidifies in 5 min. The solidification time in min for a cube of the same material,…
- GATE 2026 ME · Q30In relation to metal casting defects, match the following | Defect | | Description | | | :--- | :--- | :---…
- GATE 2025 ME · Q34A liquid metal is poured in a mold cavity of size 200 mm × 200 mm × 200 mm. The cooling is uniform in all…
Question from the official GATE 2014 ME paper (Set 3), IIT Kharagpur. Solutions by PARIXO AI. All 65 questions of this paper.